AWS B2. 1-8-025-2001, Standard Welding Procedure Specification (WPS) for Gas Tungsten Arc Welding Followed by Shielded Metal Arc Welding of Austenitic Stainless Steel (M-8/P-8/S-8, Group 1), 1/8 Through 1-1/2 Inch Thick, ER3XX and 3XX-XX, As-Welded Condition, Primarily Plate and Structural Applications

AWS B2. 1-8-025-2001, Standard Welding Procedure Specification (WPS) for Gas Tungsten Arc Welding Followed by Shielded Metal Arc Welding of Austenitic Stainless Steel (M-8/P-8/S-8, Group 1), 1/8 Through 1-1/2 Inch Thick, ER3XX and 3XX-XX, As-Welded Condition, Primarily Plate and Structural Applications
Author :
Publisher :
Total Pages :
Release :
ISBN-10 : 0871716941
ISBN-13 : 9780871716941
Rating : 4/5 (941 Downloads)

Book Synopsis AWS B2. 1-8-025-2001, Standard Welding Procedure Specification (WPS) for Gas Tungsten Arc Welding Followed by Shielded Metal Arc Welding of Austenitic Stainless Steel (M-8/P-8/S-8, Group 1), 1/8 Through 1-1/2 Inch Thick, ER3XX and 3XX-XX, As-Welded Condition, Primarily Plate and Structural Applications by : American Welding Society

Download or read book AWS B2. 1-8-025-2001, Standard Welding Procedure Specification (WPS) for Gas Tungsten Arc Welding Followed by Shielded Metal Arc Welding of Austenitic Stainless Steel (M-8/P-8/S-8, Group 1), 1/8 Through 1-1/2 Inch Thick, ER3XX and 3XX-XX, As-Welded Condition, Primarily Plate and Structural Applications written by American Welding Society and published by . This book was released on 2001-01-01 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:

AWS B2. 1-8-025-2001, Standard Welding Procedure Specification (WPS) for Gas Tungsten Arc Welding Followed by Shielded Metal Arc Welding of Austenitic Stainless Steel (M-8/P-8/S-8, Group 1), 1/8 Through 1-1/2 Inch Thick, ER3XX and 3XX-XX, As-Welded Condition, Primarily Plate and Structural Applications Related Books

Standard Welding Procedure Specification (WPS) Gas Tungsten Arc Welding of Austenitic Stainless Steel
Language: en
Pages: 12
Authors: American Welding Society. Committee on Welding Qualification
Categories: Austenitic stainless steel
Type: BOOK - Published: 1994 - Publisher: